| Elemento ng haluang metal 5754 |
Nilalaman (%) |
| Aluminyo (Al) |
Balanse |
| Magnesium(Mg) |
4.0-4.9 |
| Manganese(Mn) |
0.40-1.0 |
| Silicon (Si) |
≤0.40 |
| Bakal(Fe) | ≤0.40 |
| Sink(Zn) | ≤0.25 |
| Copper(Cu) | ≤0.10 |
| Chromium(Cr) | 0.05-0.25 |
| Titanium(Ti) | ≤0.20 |
| Iba pa(bawat isa) | ≤0.05 |
| Kabuuang mga Dumi | ≤0.15 |
| Ari-arian ng haluang metal 5754 |
Galit: O |
Galit: H12/H32 | Galit: H14/H34 | Galit: H16/H36 | Galit: H18/H38 |
| Lakas ng makunat |
195-240MPa |
220-260 MPa | 245-285 MPa | 270-310 MPa | 295 -335 MPa |
| Lakas ng Yield (0.2% offset) |
80-120 MPa |
165-200 MPa | 205-240 MPa | 230-270MPa | 260-300 MPa |
| Pagpahaba sa Break |
22-28% |
16-20% | 12-16% | 8-12% | 6-10% |
| Katigasan (Rockwell B) |
Walang pagpapatigas sa trabaho |
Mababa | Katamtaman | Mataas | Napakataas |
| Ari-arian ng haluang metal 5754 |
Halaga |
| Densidad |
2.48 g/cm³ |
| Punto ng Pagkatunaw |
527–621°C |
| Thermal Conductivity |
190-225 W/m·K |
| Electrical Conductivity |
30-40% IACS |
| Thermal Expansion Coefficient |
13.1-13.3×10⁻⁶/°C (20–100°C) |
| Modulus ng Elasticity | 69GPa |
| Rate ni Poisson | 0.33 |
| Tiyak na Kapasidad ng init | 0.22 BTU/(lb·°F) (920 J/(kg·°C)) |
| Shear Modulus | 26 GPa |
| Bulk Modulus | 69 GPa |
| ASTM |
B209, B479 . |
| ISO |
ISO 26204 , ISO 6892, ISO 9001, ISO 14001. |
| UNS |
A91060. |