| Elemento ng haluang metal 3003 |
Nilalaman (%) |
| Aluminyo (Al) |
97.0-98.5 |
| Manganese(Mn) |
1.0-1.5 |
| Silicon(Si) |
≤0.6 |
| Bakal(Fe) |
≤0.05 |
| Cooper(Cu) | ≤0.05 |
| Sink(Zn) | ≤0.10 |
| Iba pang Elemento | ≤0.05 |
| Kabuuang mga Dumi | ≤0.35 |
| Pag-aari ng haluang metal 3003 |
Karaniwang Halaga (Temper: O) |
Karaniwang Halaga (Temper: H12) |
Karaniwang Halaga (Temper: H14) |
Karaniwang Halaga (Temper: H16) |
Karaniwang Halaga (Temper: H18) |
| Lakas ng makunat |
90-140 MPa |
140-185 Mpa | 165-205Mpa | 185-225Mpa | ≥215Mpa |
| Lakas ng Yield (0.2% offset) |
≤55 MPa |
110-145 MPa | 135-170 MPa | 160-195 MPa | ≥185Mpa |
| Pagpahaba sa Break |
20-25% |
8-12% | 6-10% | 4-8% | 3-6% |
| Katigasan (Rockwell B) |
35-45HB |
35-45HB | 45-65HB | 55-75HB | 65-85HB |
| Ari-arian |
Halaga |
| Densidad |
2.7 g/cm³ |
| Punto ng Pagkatunaw |
643–657°C |
| Thermal Conductivity |
209 W/m·K |
| Electrical Conductivity |
61% IACS |
| Thermal Expansion Coefficient |
23.1×10⁻⁶/°C (20–100°C) |
| ASTM |
B209 (sheet/plate), B221 (extrusions), B233 (wire), B479 (foil). |
| ISO |
ISO 26204 (alloy designations), ISO 6892 (mechanical testing). |
| UNS |
A91060 (United States Numbering System). |