Elemento |
Nilalaman (%) |
Aluminyo (Al) |
≥97.5 |
Silicon (Si) |
0.5-0.9 |
Bakal (Fe) |
0.6-1.0 |
Manganese(Mn) |
≤0.20 |
| Copper(Cu) | ≤0.10 |
| Sink(Zn) | ≤0.10 |
| Tatanium(Ti) | ≤0.08 |
| Chromium(Cr) | ≤0.05 |
| Nikel(Ni) | ≤0.05 |
| Mataba(Pb) | ≤0.05 |
| Ari-arian |
Karaniwang Halaga (Temper: O) |
| Lakas ng makunat |
60–100 MPa |
| Lakas ng Yield (0.2% offset) |
20–50 MPa |
| Pagpahaba sa Break |
1.0–3.0% |
| Katigasan (Rockwell B) |
18–30HV |
| Ari-arian |
Halaga |
| Densidad |
2.7 g/cm³ |
| Punto ng Pagkatunaw |
643–657°C |
| Thermal Conductivity |
205 W/m·K |
| Electrical Conductivity |
61% IACS |
| Thermal Expansion Coefficient |
23.1×10⁻⁶/°C (20–100°C) |
| ASTM |
ASTM B479,FDA 21 CFR 175.300,FDA 21 CFR 177 |
| ISO |
ISO 26204 (alloy designations), ISO 6892 (mechanical testing), ISO 9001, ISO 14001. |
| EN |
EN 546,EC No 1935/2004 |