Element | Content (%) |
Aluminum (Al) | ≥98.5 |
Silicon (Si) | 0.5-0.9 |
Iron (Fe) | 0.6-1.0 |
Copper(Cu) | ≤0.15 |
Manganese(Mn) | ≤0.10 |
Magnesium(Mg) | ≤0.05 |
Zinc(Zn) | ≤0.10 |
Other Impurities | ≤0.15(total) |
Property | Temper: O | Temper: 12 | Temper: 14 | Temper: 16 | Temper: 18 |
Tensile Strength | 90-130 MPa | 110-150 MPa | 130-170 MPa | 150-190 MPa | ≥170 MPa |
Yield Strength (0.2% offset) | 35-65 MPa | 65-105 MPa | 95-135 MPa | 125-165 MPa | ≥150 MPa |
Elongation at Break | 18-25% | 8-14% | 6-12% | 4-10% | 3-8% |
Hardness (Rockwell B) | 25-40 | 40-55 | 50-70 | 60-80 | 70-90 |
Property | Value |
Density | 2.7 g/cm³ |
Melting Point | 643–657°C |
Thermal Conductivity | 209 W/m·K |
Electrical Conductivity | 61% IACS |
Thermal Expansion Coefficient | 23.1×10⁻⁶/°C (20–100°C) |
ASTM | B209 (sheet/plate), B221 (extrusions), B233 (wire), B479 (foil). |
ISO | ISO 26204 (alloy designations), ISO 6892 (mechanical testing). |
UNS | A91060 (United States Numbering System). |