AA3105-H26 Painted Aluminum Strip for Sign Making
You are here: Home » Brushed Surface » By Shape » Prepainted Aluminum Strip » AA3105-H26 Painted Aluminum Strip for Sign Making

loading

Share to:
facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
sharethis sharing button

AA3105-H26 Painted Aluminum Strip for Sign Making

AA3105-H26 painted aluminum strip in 0.4–3.0mm combines good rigidity, flatness and color consistency for sign panels, display boards, logo plates and other fabricated signage components.
  • AA3105

  • Dingang

  • 7606125900

Availability:
Quantity:

AA3105-H26 Painted Aluminum Strip for Sign Making

AA3105-H26 painted aluminum strip is a color-coated aluminum material for advertising panels, logo boards, sign cabinets, display panels, backing plates and other fabricated signage requiring useful rigidity, flatness, corrosion resistance and consistent surface appearance.

The available product range covers approximately 0.4mm to 3.0mm thickness and 20mm to 1250mm width. Narrow slit material can be supplied for selected sign components, while wider material is suitable for flat panels, cabinet components and fabricated advertising structures.

PE polyester coating is available for general indoor and outdoor signage, while PVDF coating can be specified where stronger long-term UV and weathering performance is required. Colors, gloss, coating sides and protective film can be configured according to project requirements.

H26 provides greater strength and stiffness than softer 3105 tempers but has limited elongation. Tight bends, channel-letter returns and complex formed components should therefore be evaluated according to material thickness, bend radius, coating flexibility and fabrication equipment before bulk production.

Request a Quotation

AA3105 H26 painted aluminum strip for advertising sign making

AA3105-H26 Painted Aluminum Strip Specifications

Parameter

Available Specification

Application Guidance

Product

Painted Aluminum Strip / Sheet

For advertising panels, logo boards, display panels and fabricated signage

Alloy

AA3105 / EN AW-3105

Al-Mn-Mg alloy widely used for painted and fabricated aluminum products

Temper

H26

Higher stiffness with less forming margin than H22 or H24

Thickness

0.4–3.0 mm

Select according to sign type, panel dimensions and fabrication method

Thickness Tolerance

Project-Specific

Required tolerance should be confirmed for the exact gauge before production

Width

20–1250 mm

Narrow slitting for strip applications and wider material for sign panels

PE Coating

Available

General signage, displays and moderate exterior exposure

PVDF Coating

Optional

For more demanding exterior UV and weathering requirements

Coating Thickness

Typically 18–28 μm according to coating system

PE and PVDF film thickness should be specified separately

Coating Sides

Single-Side / Double-Side / Top Coat + Back Coat

Reverse-side finish should be defined where visible after fabrication

Finish

Gloss / Matte / Metallic / Custom

Gloss and surface appearance should be approved with the required color

Colors

RAL / PANTONE / Approved Physical Sample

Brand-critical colors should be approved using a production sample

Reference Tensile Strength

Approx. 175–225 MPa

Reference range for EN AW-3105 H26

Reference 0.2% Proof Strength

Approx. ≥150 MPa

Final contractual value should follow the specified material standard

Reference Elongation

Approx. ≥3%

H26 should not be treated as a high-elongation deep-forming temper

Core ID

76 / 152 mm or Custom

Confirm against slitting, unwinding or bending equipment

Protective Film

Optional

Useful during routing, cutting, printing, bending and transport

Substrate Standard

ASTM B209 / EN 485 when specified

Relevant to alloy, temper, mechanical properties and dimensions

Coil-Coated Product Standard

EN 1396 when specified

Relevant to coating system, color, gloss, adhesion and coated-product requirements

MOQ

Approx. 1 ton for applicable specifications

Special colors and very narrow widths may require different minimum quantities

Lead Time

Approx. 15–25 working days

Final schedule depends on coating, color, dimensions and quantity

Mechanical values above are reference values for AA3105-H26. Where mechanical properties are contractual requirements, the applicable material standard, thickness range and batch-specific inspection documentation should be agreed before production.

Send Your Sign Aluminum Specification

Why Choose AA3105-H26 for Sign Panels?

AA3105-H26 provides greater stiffness than softer 3000-series tempers. This makes it useful for flat panels, logo plates, sign-cabinet components and backing plates where dimensional stability is more important than severe forming.

Panel Rigidity

Higher H26 strength helps reduce handling deformation and can provide better rigidity for flat sign components at the same material thickness.

Flatness and Dimensional Stability

Controlled flatness is important for vinyl application, direct printing, routing and visible sign panels where waviness can affect finished appearance.

Limited Forming Margin

H26 provides lower elongation than H22 or H24. Very tight bends, deep drawing and severe channel-letter corners should therefore be trialed before production.

Choosing Thickness for Sign Making

Thickness Range

Typical Application Direction

Fabrication Consideration

0.4–0.8 mm

Narrow strip, lightweight sign components and selected letter parts

Bend radius, feeding and coating flexibility should be checked

0.8–1.5 mm

Sign cabinets, backing panels, logo plates and fabricated signage

Useful balance of panel rigidity and fabrication capability

1.5–2.0 mm

Larger rigid sign panels and dimensional components

Higher bending force and larger bend radius are normally required

2.0–3.0 mm

Heavy flat panels, fabricated plates and rigid sign components

Normally not used as thin automatic channel-letter return coil

Painted Sign Sheet vs Channel Letter Coil

Painted sheet for flat advertising panels and narrow aluminum coil for channel-letter returns belong to the same signage material family but have different fabrication requirements.

Feature

Flat Sign Panel Material

Channel Letter Return Coil

Primary Requirement

Flatness and panel stiffness

Repeatable bending and machine feeding

Thickness Direction

Application-specific and often thicker

Commonly thinner strip selected around the bending system

Width

Wide sheet or strip

Narrow strip matched to letter-return depth

Temper Priority

Rigidity and flatness can be prioritized

Formability and springback control are critical

Main Processes

Cutting, routing, punching and riveting

Notching, bending, flanging and seaming

For automatic channel-letter bending, buyers should provide the machine manufacturer and model, strip thickness, required return depth, coil ID, maximum coil OD and minimum bend radius before final material selection.

PE vs PVDF Coating for Signage

Feature

PE Polyester

PVDF

Positioning

Economical general-purpose sign coating

Higher-performance exterior coating

Typical Use

Indoor displays and general outdoor signs

Long-exposure exterior signage and architectural graphics

UV Resistance

Depends on resin and pigment quality

Generally stronger for demanding exterior exposure

Color Retention

Project-specific

Preferred where long-term exterior appearance is important

Cost

Lower

Higher

PE and PVDF should not be assigned a universal number of outdoor service years. Actual durability depends on pretreatment, primer, coating chemistry, pigment, dry-film thickness, sign orientation, climate, UV exposure and maintenance.

Graphic and Printing Compatibility

Painted aluminum used in signage is often required to accept vinyl graphics, screen printing or UV flatbed printing. Compatibility should be verified using the actual coating and graphic system rather than assuming every painted surface behaves the same.

Vinyl Graphics

Pressure-sensitive vinyl should be applied to a clean, dry surface free from oil, silicone, dust and processing contamination. A representative adhesion trial is recommended when a new paint and vinyl combination is introduced.

UV Flatbed Printing

UV-curable ink adhesion can vary with coating chemistry, gloss and surface treatment. Test printing and adhesion evaluation are recommended before large production runs.

Screen Printing

Screen-print systems should be evaluated for adhesion and curing compatibility with the selected painted aluminum finish.

Protective Film

Removable protective film can be specified to reduce scratching during routing, cutting, transport and handling. Film type and removal timing should be compatible with the coating.

Color Matching for Corporate Signage

Corporate and retail signage frequently requires repeatable brand colors across multiple locations or production batches.

RAL and PANTONE Matching

RAL, PANTONE or an approved physical color sample can be used as a reference subject to pigment and coating feasibility.

Color Difference

Large sign programs can define a master sample, measurement method and acceptable ΔE tolerance for batch-to-batch consistency.

Gloss Control

Gloss should be controlled together with color because panels with similar color readings can still look different when installed side by side if their gloss levels vary.

Metallic and Directional Colors

Metallic and effect colors can change appearance with viewing angle and material orientation. A production sample should be approved before a large order.

Traffic Sign Applications Require Separate Verification

AA3105 painted aluminum can be suitable for general parking signs, property signs, commercial directional panels and information signage where the project specification permits.

Regulated highway traffic signs can require specific aluminum alloys, thicknesses, surface preparation, conversion treatment and approved retroreflective sheeting. A general AA3105-H26 painted strip should therefore not automatically be described as compliant highway-sign material.

For regulated road-sign projects, the applicable national, state or municipal specification should be provided before material selection.

EN 1396 for Coil-Coated Aluminum

EN 1396:2023 applies specifically to coil-coated wrought aluminum sheet and strip for general applications, including material that is coated in master-coil form and subsequently slit into narrow strip.

Purchase specifications can define the aluminum alloy and temper, substrate thickness, width, coil dimensions, coating system, top-side color, nominal gloss, reverse coating and protective film.

Coating tests can include dry-film thickness, gloss and color difference, while additional adhesion, bend and durability criteria can be agreed between supplier and purchaser.

Fabrication Methods

Slitting

AA3105-H26 can be slit into narrow strips for sign components. Width tolerance, camber and edge burr should be controlled where the material feeds through automated equipment.

Shearing and Cutting

Painted aluminum can be cut using suitable sheet-metal tools. Clean tooling helps reduce edge deformation and surface scratching.

CNC Routing

Wider painted sheet can be CNC routed for letters, logos and custom panel shapes using tooling and feed conditions suitable for aluminum.

Punching

Mounting holes, slots and other features can be punched when die clearance and tooling are appropriate for the selected material thickness.

Bending

H26 can be bent, but minimum bend radius should reflect material thickness, bend orientation and coating flexibility. Very tight folds should not be assumed suitable across the entire 0.4–3.0mm range.

Riveting and Mechanical Assembly

Painted aluminum panels can be assembled with compatible rivets and fasteners. Outdoor installations should consider galvanic compatibility between aluminum and adjacent hardware.

Welding

AA3105 is weldable, but organic paint normally must be removed from the weld zone. Heat can discolor or damage nearby coating, so post-weld refinishing may be required.

Flatness for Sign Panels

Flatness is an important purchasing parameter for wide advertising panels because waviness can remain visible after vinyl application, direct printing or installation under directional lighting.

Buyers requiring large-format panels can specify maximum flatness deviation together with thickness, width and surface-finish requirements.

Outdoor Sign Durability

Outdoor sign durability depends on the entire coated system rather than only the aluminum alloy or the words PE and PVDF.

Pretreatment, primer, coating chemistry, pigment, film thickness, UV exposure, sign orientation, pollution, coastal salt, fabrication and maintenance can all affect color and film integrity.

Any coating warranty should therefore apply to the exact coating construction and defined environmental exposure rather than a generic resin name.

Signage Applications

  • Flat advertising sign panels

  • Commercial logo boards

  • Storefront signage

  • Sign-cabinet faces and backing components

  • Channel-letter back plates

  • Selected channel-letter side strips after forming trials

  • Wayfinding signs

  • Parking and property signs

  • Safety and information signs

  • Retail display panels

  • Exhibition display systems

  • Decorative brand panels

  • CNC-cut aluminum sign components

Regulated highway signs, structural facade panels and specialized engineered signage should be reviewed against their applicable project specifications before material selection.

painted aluminum strip application for advertising signs

Quality Control Requirements

Alloy and Temper

AA3105-H26 should be verified against the agreed material specification where mechanical properties are contractual.

Base-Metal Thickness

Aluminum thickness should be measured separately from the organic coating and controlled against the agreed tolerance.

Width and Edge Quality

Narrow strip should maintain controlled width, camber and burr where it will be used in automated feeding or forming equipment.

Flatness

Flatness can be specified for wide panel material where visible waviness would affect printed graphics or installed appearance.

Dry-Film Thickness

PE or PVDF coating thickness should be measured against the agreed coating construction rather than applying one universal value to every paint system.

Coating Adhesion

Cross-hatch or another agreed test can be used to evaluate coating adhesion to the pretreated aluminum substrate.

T-Bend / Bend Test

Where bending is required, coating flexibility should be tested at a severity representative of the finished component.

Color Difference

Brand signage programs can specify a master sample, measurement geometry and acceptable color-difference tolerance.

Gloss

Gloss should be controlled with color where multiple sign panels or locations must maintain a consistent appearance.

Graphic Adhesion Trial

Vinyl, reflective sheeting, UV ink and screen-print applications should be validated with the actual painted surface before mass production.

Information Required for a Quotation

For accurate material selection and pricing, please provide:

  • Final sign application

  • Required thickness

  • Required width

  • Strip or wide-sheet format

  • PE or PVDF coating

  • Single-side, double-side or top/back coating

  • Required dry-film thickness

  • RAL, PANTONE or physical color reference

  • Gloss or matte requirement

  • Flatness requirement

  • Bend or T-bend requirement

  • Vinyl, reflective film or direct-print system

  • Automatic bending-machine model where applicable

  • Minimum bend radius

  • Core ID

  • Maximum coil OD and coil weight

  • Protective-film requirement

  • Required substrate standard

  • Required coating tests

  • Required material or inspection documentation

  • Order quantity

  • Destination market

Get a Custom Sign Aluminum Proposal

Frequently Asked Questions

What is AA3105-H26 painted aluminum strip used for?

It is used for advertising panels, logo boards, sign cabinets, display panels, backing plates, wayfinding signs and other fabricated signage requiring useful rigidity and a factory-painted finish.

Why use H26 temper for sign panels?

H26 provides greater strength and stiffness than softer tempers, helping flat panels retain shape. The tradeoff is lower elongation and reduced tolerance for very tight bending.

What is the tensile strength of AA3105-H26?

A commonly published EN AW-3105 H26 reference range is approximately 175–225 MPa, with minimum 0.2% proof strength around 150 MPa.

Is the elongation of AA3105-H26 10%?

A universal 10% minimum should not be specified for H26. Published EN AW-3105 H26 data gives approximately 3% minimum elongation for common thin-sheet thickness ranges.

Can H26 aluminum be bent?

Yes, but bend radius should be selected according to material thickness, bend direction and coating flexibility. Tight corners should be tested using the actual material before mass production.

Is H26 suitable for automatic channel-letter bending?

It can be suitable for selected profiles and machines, but channel-letter fabrication normally prioritizes formability. Machine model, strip thickness, width, return depth and minimum bend radius should be confirmed before ordering.

Is 2–3mm material suitable for channel-letter returns?

It is generally more appropriate for rigid panels or fabricated structural sign components. Channel-letter returns normally use thinner material selected around the bending equipment and letter construction.

Can the surface accept vinyl graphics?

Yes, when the selected coating is suitable. An adhesion test using the actual vinyl and painted surface is recommended before high-volume production.

Can it be UV flatbed printed?

Yes, subject to ink and surface compatibility. A representative print and adhesion test should be completed before commercial production.

Can the sheet be screen printed?

Suitable painted aluminum can be screen printed, but ink chemistry, curing conditions and coating surface should be validated together.

Can reflective sheeting be applied?

Reflective sheeting can be evaluated, but adhesion depends on surface preparation and the film system. The reflective-sheeting manufacturer's application instructions should be followed.

Is AA3105-H26 automatically suitable for highway traffic signs?

No. Regulated highway signs can require specific alloys, thicknesses, surface treatment and approved reflective materials. The governing road-sign specification should be checked before material selection.

What is the difference between PE and PVDF?

PE polyester is generally more economical for indoor and standard outdoor signage, while PVDF is commonly selected for more demanding exterior UV and weathering exposure.

How long will PE or PVDF coating last outdoors?

There is no universal service-life figure. Performance depends on pretreatment, coating formulation, pigment, film thickness, UV exposure, climate, sign orientation and maintenance.

Can custom corporate colors be matched?

Yes. RAL, PANTONE or approved physical samples can be used as color references subject to coating and pigment feasibility.

Can both sides be painted?

Yes. Single-side, double-side and top-coat plus back-coat configurations can be discussed. Reverse-side color should be specified where it remains visible.

Can protective film be supplied?

Yes. Protective film can be supplied for compatible finishes to reduce scratching during cutting, routing, transport and fabrication.

Can AA3105 be welded?

Yes. The aluminum substrate is weldable, but paint normally needs to be removed from the weld zone and the affected area may require refinishing after welding.

What is EN 1396?

EN 1396 specifies requirements for coil-coated aluminum sheet and strip, including substrate information, dimensions, coating system, color, gloss and relevant coating tests.

What is the MOQ?

The current program lists approximately 1 ton for applicable specifications. Special colors, widths or coating systems may require a different minimum quantity.

What is the typical lead time?

The current program lists approximately 15–25 working days. Actual timing depends on color matching, coating system, slitting dimensions and order quantity.

What information is required for an accurate quotation?

Please provide thickness, width, sign application, PE or PVDF coating, color, gloss, coating sides, printing or vinyl system, bend requirements, coil dimensions, quantity, required documentation and destination.

Should samples be tested before bulk production?

Yes. New colors, tight bending, automatic channel-letter equipment, reflective films, vinyl systems and direct-print applications should be validated using representative samples before commercial production.

Contact Dingang for Samples and Pricing

Previous: 
Next: 

Product Category

Consult Us To Get Your Customized Aluminum Solution

We help you specify and source the coated aluminum you need, on time and within budget.

Products

Application

Quick links

Follow Us

Contact Us

    joey@cnchangsong.com
    +86-18602595888
   Building 2, Zhixing Business Plaza, No.25 North Street, Zhonglou District, Changzhou City, Jiangsu Province, China
    Chaoyang road, Konggang economic development area, Lianshui, Huai'an city, Jiangsu,China
© COPYRIGHT 2026 CHANGZHOU DINGANG METAL MATERIAL CO., LTD. ALL RIGHTS RESERVED.